Polymer Property : Glow Wire Test = 1430 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1...
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific)
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East)
Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market.
Glow Wire Test 775 °C
1430 °F
GWIT
PTS Tristar® PC-10R-(V20) 20 MFI UV Stabilized Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 775 °C
1430 °F
GWIT
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Glow Wire Test 775 °C
1430 °F
GWIT
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 775 °C
1430 °F
GWIT
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 775 °C
1430 °F
GWIT
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 775 - 960 °C
1430 - 1760 °F
Average value: 868 °C Grade Count:8
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL PX9406P PPE
NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color.
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific)
Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East)
Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Europe-Africa-Middle East)
Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCD933 PPE-TPE
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific)
Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a..
Glow Wire Test 775 °C

@Thickness 0.800 mm
1430 °F

@Thickness 0.0315 in
IEC 60695-2-13
RTP Company RTP 299 X 117593 C Nylon 6/6 (PA) Glass Fiber - Flame Retardant - Halogen Free