Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 923X PC (Asia Pacific) Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East) Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 923X PC Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 940 PC (Europe-Africa-Middle East) LEXAN 940 is a medium viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Glow Wire Test | 825 - 960 °C | 1520 - 1760 °F | IEC 60695-2-13 |
SABIC Innovative Plastics LNP LUBRICOMP OFL38A PPS - Branched (Europe-Africa-Middle East) LNP* LUBRICOMP* OFL38A is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features include : Internally Lubricated. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics LNP THERMOCOMP UX06032 PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UX06032 is a compound based on Polyphthalamide resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Non-Brominated & Non-Chlorin.. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |