Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCP821U PPE-TPE (Asia Pacific) UV stabilized, halogen free Flexible Noryl injection molding grade for overmolding applications such as plugs, strain relief's, and connectors. Good color stability after UV weathering per ASTM D445.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Valox® 457 PBT 6.5% GR PBT, UL94 V-0/5V. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Glow Wire Test | 725 °C | 1340 °F | Ignition Temperature; ISO 60695-2-13 |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T.. |
|||
Glow Wire Test | 725 °C | 1340 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |