Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -40.0 - 60.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® RCY6113 PC+ABS (Asia Pacific)
Cycoloy* RCY6113 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 5VB rating @ 2.0mm an..
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DBL34E PC (Europe-Africa-Middle East)
LNP* LUBRICOMP DBL34E is a compound based on Polycarbonate resin containing Glass Bead, PTFE. Added features include: Easy Molding, Internally Lubricated.
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC (Europe-Africa-Middle East)
LNP* LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features include; Internally Lubricated, Easy Molding.
CTE, linear, Transverse to Flow 76.0 - 100 µm/m-°C

@Temperature 55.0 - 260 °C
42.2 - 55.6 µin/in-°F

@Temperature 131 - 500 °F
Average value: 83.8 µm/m-°C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear, Transverse to Flow 76.0 - 100 µm/m-°C

@Thickness 2.00 - 4.00 mm
42.2 - 55.6 µin/in-°F

@Thickness 0.0787 - 0.157 in
Average value: 83.8 µm/m-°C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC
LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare.
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RCL34 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP REL22 PA 66
LNP* LUBRICOMP* REL22 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Electrically Conductive.
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A..
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRILOY D2000 PC
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE)
LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber.
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP NX11302 PC+ABS (Asia Pacific)
This is a PC/ABS compound with colorable, good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature 20.0 °C
42.2 µin/in-°F

@Temperature 68.0 °F
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend
Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sepa..
CTE, linear, Transverse to Flow 76.0 µm/m-°C
42.2 µin/in-°F
z, below Tg; IPC TM-650 2.4.24
Arlon 37N Polyimide Low-Flow
37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir..
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature 20.0 °C
42.2 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® RS 60M10E5 Nylon 6 Alloy, 10% Mineral Filled (Conditioned)
RS 60 series rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents). Stability of mechanical, electrical and dimensional properties.Mineral filled..
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DFL44 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DFL44 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE.
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON MV006BS PP
LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl..
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
42.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC
LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated.