SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features include; Internally Lubricated, Easy Molding.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Water Absorption 0.11 %

@Time 86400 sec
0.11 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0016 cm/cm
0.0016 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 118 MPa
17100 psi
5 mm/min; ISO 527
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
2.9 %
2.9 %
Flexural Strain, break, 2 mm/min; ISO 178
Tensile Modulus 8.40 GPa
1220 ksi
1 mm/min; ISO 527
Flexural Strength 176 MPa
25500 psi
2 mm/min; ISO 178
Flexural Yield Strength 177 MPa
25700 psi
2 mm/min; ISO 178
Flexural Modulus 8.10 GPa
1170 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 24.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
13.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af