Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DFL44 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DFL44 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* DFL44 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 86.0 MPa
12500 psi
5 mm/min; ISO 527
Elongation at Break 2.3 %
2.3 %
5 mm/min; ISO 527
Tensile Modulus 6.40 GPa
928 ksi
1 mm/min; ISO 527
Flexural Yield Strength 127 MPa
18400 psi
2 mm/min; ISO 178
Flexural Modulus 4.90 GPa
711 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 26.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
14.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 76.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 147 °C
297 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af