Polymer Property : Glass Transition Temp, Tg = 225 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -27.0 - 225 °C
-16.6 - 437 °F
Average value: 100 °C Grade Count:82
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Glass Transition Temp, Tg 220 - 225 °C
428 - 437 °F
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof..