Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer Solvay Specialty Polymers
Trade Name Veradel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other solid particles. The grades differ by their molecular weights, with 3000P the highest and 3600P the lowest. There is a direct correlation between molecular weight and solution viscosity.PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water, and mineral acids. Cast films or coatings of PESU are transparent and have additional desirable properties including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance.Features: Acid Resistant; Flame Retardant; Good Adhesion; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium RigidityUses: Adhesives; Coating Applications; CompoundingAdditional Properties: Residual Solvent - Internal Method 0.50 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ISO 62
Viscosity 370 cP
370 cP
Solution Viscosity; ASTM D455
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 49.0 µm/m-°C
27.2 µin/in-°F
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Compliance Properties Metric English Comments
NSF Yes
Yes
NSF 51
Descriptive Properties Value Comments
Agency Ratings NSF 51
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Transparent - Slight Yellow
Form Granules; Powder
Processing Technique Coating; Solution Processing; Spraying