Material Notes:
Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing into solutions and to improve adhesion to substrates when used as a coating. Veradel 3600RP r-PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water and mineral acids. Cast films or coatings of r-PESU are transparent and have additional desirable properties, including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance. Veradel r-PESU polymers are available in two molecular weight regimes. Veradel® 3000RP is a high molecular weight sulfone polymer with a relatively low level of functionality while Veradel 3600RP has a lower molecular weight sulfone polymer (approximately half the molecular weight of the Veradel 3000RP) with roughly 3-5 times higher level of functionality. The differences in molecular weight results in highly varied levels of viscosity, when measured under similar conditions. Typical applications include high-temperature coating formulations and specialty adhesives. All Veradel r-PESU polymers are produced at Solvay's state-of-the-art, world-scale facility in Panoli, India under ISO 9001:2000 and ISO 14001:2004 certified quality management systems.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium 1.5 %
1.5 %
Measured at time of packing; Internal Method
Particle Size 250 µm
250 µm
D50 Sieve measurement; Internal Method
Viscosity 80 cP

@Temperature 40.0 °C
80 cP

@Temperature 104 °F
35% solution in DMAc (measured at 35% solids); Internal Method
560 cP

@Temperature 40.0 °C
560 cP

@Temperature 104 °F
35% solution in DMAc (measured at 35% solids); Internal Method
Mechanical Properties Metric English Comments
Tensile Strength 90.0 MPa
13100 psi
ASTM D638
Elongation at Yield 6.5 %
6.5 %
ASTM D638
Tensile Modulus 2.70 GPa
392 ksi
ASTM D638
Flexural Strength 2.60 MPa
377 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 220 °C
428 °F
DSC
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Chemical Properties Metric English Comments
Carboxyl End Groups 170 meq/kg
170 meq/kg
Titration; Internal Method
Descriptive Properties Value Comments
Agency Ratings NSF 51
Maximum Temperature of Use: 124°C (356°F)
Appearance Transparent - Slight Yellow
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Acid Resistant
Flame Retardant
Good Adhesion
Good Chemical Resistance
Good Creep Resistance
Good Dimensional Stability
Good Thermal Stability
Good Toughness
High Flow
High Heat Resistance
High Tensile Strength
Hydrolysis Resistant
Low Molecular Weight
Medium Rigidity
Forms Granules
Powder
Generic PESU
Processing Method Coating
Solution Processing
Spraying
Residual Solvent (%) 1.5
Gas Chromatography
Uses Adhesives
Binder
Coating Applications
Users viewing this material also viewed the following: