Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.40 g/cc
0.267 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.6 MPa
7200 psi
Elongation at Break 19.3 %
19.3 %
Modulus of Elasticity 16.6 GPa
2410 ksi
Thermal Properties Metric English Comments
Melting Point 217 - 220 °C
423 - 428 °F
Solidus 217 °C
423 °F
Liquidus 220 °C
428 °F
Component Elements Properties Metric English Comments
Copper, Cu 0.50 %
0.50 %
Silver, Ag 3.0 %
3.0 %
Tin, Sn 96.5 %
96.5 %