Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 217 °C | 423 °F | (Dry) |
Radici Radilon® S 38M (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Melting Point | 217 °C | 423 °F | |
Radici Radilon® S 38M (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Melting Point | 217 °C | 423 °F | ISO 1135 7-1-3 |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Melting Point | 217 °C | 423 °F | |
Nihon Superior SN96Cl Lead-Free Solder Alloy |
|||
Melting Point | 217 °C | 423 °F | Peak |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 217 - 225 °C | 423 - 437 °F | |
Indium Corp. Indalloy 251 Tin Solder Alloy Castin Patented alloyInformation Provided by Indium Corporation |
|||
Melting Point | 217 °C | 423 °F | Eutectic |
Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy Multicore promoted alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 217 °C | 423 °F | Eutectic |
Indium Corp. Indalloy® 246 95.5Sn/4.0Ag/0.5Cu Lead-Free Solder Alloy Petzow (German) prior art reference makes this alloy patent-free.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 217 °C | 423 °F | Eutectic |
Indium Corp. Indalloy® 252 95.5Sn/3.9Ag/0.6Cu Lead-Free Solder Alloy Alloy of choice for general SMT assembly. NEMI promoted alloy (average composition of Indalloy #241& #246).Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 217 - 220 °C | 423 - 428 °F | |
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 217 - 226 °C | 423 - 439 °F | |
Indium Corp. Indalloy 260 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 217 °C | 423 °F | Eutectic |
Indium Corp. Indalloy® 238 Sn-Au Solder Alloy Lower temp eutectic, in the Au Sn system.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 217 - 227 °C | 423 - 441 °F | |
Indium Corp. Indalloy® 263 Tin-Silver-Copper Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Melting Point | 217 °C | 423 °F | |
Williams Advanced Alloys WS217 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 217 °C | 423 °F | ISO 3146 |
Chengdu Polyster FH7560 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H7560 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by.. |
|||
Melting Point | 217 °C | 423 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PM471 45 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 217 °C | 423 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PM471 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | <= 217 °C | <= 423 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Melting Point | <= 217 °C | <= 423 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Melting Point | <= 217 °C | <= 423 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade) Product Description: LD 650 is an easy flowing LDPE grade with a good flexibility and excellent toughness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No.. |
|||
Melting Point | 217 °C | 422 °F | ASTM D2133 |
Ensinger Tecamid® 6/12 Nylon (PA612) Type 6/12 has lower moisture absorption rates than nylon 6/6, hence superior dimensional stability.Information provided by Ensinger, Inc. |
|||
Melting Point | 217 °C | 423 °F | 10°C/min |
Arkema Group Orgalloy® LT 4060 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrates a good balance of properties eg, high flexibility (200 MPa), good.. |
|||
Melting Point | 217 °C | 423 °F | ISO 3146 |
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
Melting Point | 217 °C | 423 °F | ISO 3146 |
Arkema Group ORGASOL® 1002 ES 4 Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
Melting Point | 217 °C | 423 °F | |
AIM CASTIN Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 217 - 218 °C | 423 - 424 °F | |
AIM SAC305 Lead-Free Solder for Photonic Packaging This alloy falls under the JEIDA recommendation for lead-free soldering. When used in wave soldering, AIM’s SAC305 bar solder offers far superior fluidity as compared to other alloys and makes of b.. |
|||
Melting Point | 217 °C | 423 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® HTR8539 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8539 is a 72 Shore D, plasticiser free, high performance resin for extrusion. It has high viscosity.Information provided by DuPont Performance Polymers |
|||
Melting Point | 217 °C | 423 °F | DAM; ASTM D3418 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 217 °C | 423 °F | DAM; ASTM D3418 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |