Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 423 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 217 °C
423 °F
(Dry)
Radici Radilon® S 38M (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Melting Point 217 °C
423 °F
Radici Radilon® S 38M (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Melting Point 217 °C
423 °F
ISO 1135 7-1-3
Radici Radilon® SLVHPL128 (dry) Nylon 6
Plasticized for improved flexibilityInformation provided by Radici group.
Melting Point 217 °C
423 °F
Nihon Superior SN96Cl Lead-Free Solder Alloy
Melting Point 217 °C
423 °F
Peak
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Melting Point 217 - 225 °C
423 - 437 °F
Indium Corp. Indalloy 251 Tin Solder Alloy
Castin Patented alloyInformation Provided by Indium Corporation
Melting Point 217 °C
423 °F
Eutectic
Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy
Multicore promoted alloy.Information provided by the manufacturer, Indium Corporation.
Melting Point 217 °C
423 °F
Eutectic
Indium Corp. Indalloy® 246 95.5Sn/4.0Ag/0.5Cu Lead-Free Solder Alloy
Petzow (German) prior art reference makes this alloy patent-free.Information provided by the manufacturer, Indium Corporation.
Melting Point 217 °C
423 °F
Eutectic
Indium Corp. Indalloy® 252 95.5Sn/3.9Ag/0.6Cu Lead-Free Solder Alloy
Alloy of choice for general SMT assembly. NEMI promoted alloy (average composition of Indalloy #241& #246).Information provided by the manufacturer, Indium Corporation.
Melting Point 217 - 220 °C
423 - 428 °F
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy
Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation.
Melting Point 217 - 226 °C
423 - 439 °F
Indium Corp. Indalloy 260 Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 217 °C
423 °F
Eutectic
Indium Corp. Indalloy® 238 Sn-Au Solder Alloy
Lower temp eutectic, in the Au Sn system.Information provided by the manufacturer, Indium Corporation.
Melting Point 217 - 227 °C
423 - 441 °F
Indium Corp. Indalloy® 263 Tin-Silver-Copper Solder Alloy
Information provided by the manufacturer, Indium Corporation of America.
Melting Point 217 °C
423 °F
Williams Advanced Alloys WS217 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 217 °C
423 °F
ISO 3146
Chengdu Polyster FH7560 Thermoplastic Polyether-ester Elastomer (TPEE)
Blend of H7560 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by..
Melting Point 217 °C
423 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® PM471 45 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point 217 °C
423 °F
10°C/min; ISO 11357-1/-3
DSM Arnitel® PM471 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melting Point <= 217 °C
<= 423 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin
Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab..
Melting Point <= 217 °C
<= 423 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin
Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab..
Melting Point <= 217 °C
<= 423 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade)
Product Description: LD 650 is an easy flowing LDPE grade with a good flexibility and excellent toughness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No..
Melting Point 217 °C
423 °F
10°C/min
Arkema Group Orgalloy® LT 4060 Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrates a good balance of properties eg, high flexibility (200 MPa), good..
Melting Point 217 °C
423 °F
ISO 3146
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
Melting Point 217 °C
423 °F
ISO 3146
Arkema Group ORGASOL® 1002 ES 4 Nat 1 Polyamide 6
Information provided by Arkema Group
Melting Point 217 °C
423 °F
AIM CASTIN Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Melting Point 217 - 218 °C
423 - 424 °F
AIM SAC305 Lead-Free Solder for Photonic Packaging
This alloy falls under the JEIDA recommendation for lead-free soldering. When used in wave soldering, AIM’s SAC305 bar solder offers far superior fluidity as compared to other alloys and makes of b..
Melting Point 217 °C
423 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® HTR8539 BK316 TPC-ET  (Unverified Data**)
Hytrel® HTR8539 is a 72 Shore D, plasticiser free, high performance resin for extrusion. It has high viscosity.Information provided by DuPont Performance Polymers
Melting Point 217 °C
423 °F
DAM; ASTM D3418
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Melting Point 217 °C
423 °F
DAM; ASTM D3418
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers