Polymer Property : Melting Point = 226 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 222 - 226 °C
432 - 439 °F
Q/NHS 501
PTS PBT-1090 PBT Resin
Information provided by PTS LLC.
Melting Point 222 - 226 °C
432 - 439 °F
10°C/min; ISO11357 (DSC)
PTS PBT-1100 PBT Resin
Information provided by PTS LLC.
Melting Point 222 - 226 °C
432 - 439 °F
ISO 11357
PTS PBT-1100A PBT Resin
Information provided by PTS LLC.
Melting Point 222 - 226 °C
432 - 439 °F
ISO 11357
PTS PBT-1100A PBT Resin
Information provided by PTS LLC.
Melting Point 221 - 226 °C
430 - 439 °F
Indium Corp. Indalloy 123 Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 217 - 226 °C
423 - 439 °F
Indium Corp. Indalloy 260 Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 218 - 226 °C
424 - 439 °F
Williams Advanced Alloys WS226 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 221 - 226 °C
430 - 439 °F
Williams Advanced Alloys WS226A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 222 - 226 °C
432 - 439 °F
10°C/min; ISO11357 (DSC)
BLUESTAR PBT 1100
PBT resin is polymerized by pure terephthalic acid (PTA) and 1,4-butanediol (1,4-BDO) through direct esterification. With well-distributed molecular weight and stable quality, PBT resin possesses go..
Melting Point 222 - 226 °C
432 - 439 °F
ISO 11357
BLUESTAR PBT 1100A
Information provided by Polymer Technology and Services, LLC (PTS).
Melting Point 222 - 226 °C
432 - 439 °F
Q/NHS 501
BLUESTAR PBT 1090
Information provided by Polymer Technology and Services, LLC (PTS).