Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 222 - 226 °C | 432 - 439 °F | Q/NHS 501 |
PTS PBT-1090 PBT Resin Information provided by PTS LLC. |
|||
Melting Point | 222 - 226 °C | 432 - 439 °F | 10°C/min; ISO11357 (DSC) |
PTS PBT-1100 PBT Resin Information provided by PTS LLC. |
|||
Melting Point | 222 - 226 °C | 432 - 439 °F | ISO 11357 |
PTS PBT-1100A PBT Resin Information provided by PTS LLC. |
|||
Melting Point | 222 - 226 °C | 432 - 439 °F | ISO 11357 |
PTS PBT-1100A PBT Resin Information provided by PTS LLC. |
|||
Melting Point | 221 - 226 °C | 430 - 439 °F | |
Indium Corp. Indalloy 123 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 217 - 226 °C | 423 - 439 °F | |
Indium Corp. Indalloy 260 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 218 - 226 °C | 424 - 439 °F | |
Williams Advanced Alloys WS226 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 221 - 226 °C | 430 - 439 °F | |
Williams Advanced Alloys WS226A Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 222 - 226 °C | 432 - 439 °F | 10°C/min; ISO11357 (DSC) |
BLUESTAR PBT 1100 PBT resin is polymerized by pure terephthalic acid (PTA) and 1,4-butanediol (1,4-BDO) through direct esterification. With well-distributed molecular weight and stable quality, PBT resin possesses go.. |
|||
Melting Point | 222 - 226 °C | 432 - 439 °F | ISO 11357 |
BLUESTAR PBT 1100A Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melting Point | 222 - 226 °C | 432 - 439 °F | Q/NHS 501 |
BLUESTAR PBT 1090 Information provided by Polymer Technology and Services, LLC (PTS). |