Chengdu Polyster FH7560 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster FH7560 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blend of H7560 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Melt Flow 5.0 - 10 g/10 min
5.0 - 10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ISO 868
Tensile Strength, Ultimate 32.0 MPa
4640 psi
ISO 527-1
Elongation at Break 280 %
280 %
ISO 527-1
Flexural Modulus 0.320 GPa
46.4 ksi
ISO 178
Tear Strength 128 kN/m
730 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 217 °C
423 °F
ISO 3146
Brittleness Temperature -50.0 °C
-58.0 °F
ISO 974