Material Notes:
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrates a good balance of properties eg, high flexibility (200 MPa), good thermal performance and ductility at low temperatures.LT 4060 : standard grade, injection molding or tubes, mandrelsISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 5.0 %
5.0 %
Moisture Absorption at Equilibrium 1.1 %
1.1 %
Humidity Absorption
Melt Flow 1.0 g/10 min

@Load 5.00 kg,
Temperature 235 °C
1.0 g/10 min

@Load 11.0 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 10 %
10 %
50 mm/min
Tensile Modulus 0.200 GPa
29.0 ksi
1 mm/min
Charpy Impact, Notched NB
NB
2.20 J/cm²

@Temperature -30.0 °C
10.5 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 217 °C
423 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V