Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolite® TPF 1211 - Unreinforced Phenolic Resin having 53 mm Norton Flow with 12% Hexamine

Category Polymer , Thermoset , Phenolic
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolite® TPF 1211 - Unreinforced Phenolic Resin having 53 mm Norton Flow with 12% Hexamine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Phenolic Resin having 53mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: Grinding WheelsInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Spiral Flow 5.30 cm
2.09 in
Thermal Properties Metric English Comments
Melting Point 94.0 °C
201 °F
TRN-14