DuPont™ Fusabond® A560 Polymer Modifier

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer DuPont
Trade Name Fusabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Fusabond® A560 Polymer Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Fusabond® A560 is a chemically modified ethylene acrylate copolymer Used as a polymer modifier
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792, ISO 1183
Melt Flow 5.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 94.0 °C
201 °F
ASTM D3418, ISO 3146
Processing Properties Metric English Comments
Processing Temperature <= 310 °C
<= 590 °F