LG Chemical SEETEC EF443 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer LG Chemical
Trade Name SEETEC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC EF443 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.928 - 0.932 g/cc
0.928 - 0.932 g/cc
ASTM D1505
Melt Flow 0.80 - 1.2 g/10 min

@Load 2.61 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.6 MPa
2840 psi
500mm/min; ASTM D638
Film Elongation at Break, MD 400 %
400 %
500 mm/min; ASTM D638
Film Elongation at Break, TD 650 %
650 %
500 mm/min; ASTM D638
Elongation at Break 650 %
650 %
500 mm/min; ASTM D638
2% Secant Modulus 0.650 GPa
94.3 ksi
500mm/min; ASTM D638
Elmendorf Tear Strength MD 220 g
220 g
ASTM D1922
Elmendorf Tear Strength TD 260 g
260 g
ASTM D1922
Dart Drop Test >= 400 g
>= 0.882 lb
ASTM D1709
Film Tensile Strength at Break, MD 30.4 MPa
4410 psi
500mm/min, Ultimate; ASTM D638
Film Tensile Strength at Break, TD 30.4 MPa
4410 psi
500mm/min, Ultimate; ASTM D638
Thermal Properties Metric English Comments
Melting Point 94.0 °C
201 °F
10°C/min; ASTM D3418
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 3.5 %
3.5 %
ASTM D1003
Gloss 105 %
105 %
45°; ASTM D2457
Copyright © lookpolymers.com All Rights Reserved