Westlake Elevate™ DA532 Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Westlake Chemical Corporation
Trade Name Elevate™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Elevate™ DA532 Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Experimental ProductDescription: Westlake DA532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low seal initiation temperature, excellent film optics, and outstanding film toughness, especially at low temperatures.Application/Uses:Low temperature sealant resin for flexible packagingLamination film Additive Packages:AA (no slip, no antiblock)XL (very high slip, medium antiblock)Information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 77.0 °C
171 °F
Freezing Point
94.0 °C
201 °F
ASTM D3418
Vicat Softening Point 69.0 °C
156 °F
ASTM D1525
Flash Point >= 343 °C
>= 649 °F
ASTM E136