Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 164 °C | 327 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Proteus® LSG HS PP - Heat Stabilized Polypropylene (ASTM Product Data Sheet) |
|||
Melting Point | 164 °C | 327 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Melting Point | 164 °C | 327 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Melting Point | 164 °C | 327 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Melting Point | 164 °C | 327 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Melting Point | 164 - 167 °C | 327 - 333 °F | ASTM D3418 |
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong.. |
|||
Melting Point | 164 °C | 327 °F | DSC; ISO 11357-1,-3 |
Inno-Comp INNOPOL® CS 1-3130 30% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-3130 is a 30% talc-filled polypropylene homopolymer compound /PP-H TD30 (ISO 1043)/. This grade is available in natural and custom colored form as well.INNOPOL® CS 1-3130 is reco.. |
|||
Melting Point | 164 °C | 327 °F | DSC; ISO 11357-1,-3 |
Inno-Comp INNOPOL® CS 2-1000 Polypropylene Block-Copolymer INNOPOL® CS 2-1000 is a polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-1000 is developed for producing injection molded automo.. |
|||
Melting Point | 164 - 167 °C | 327 - 333 °F | DSC |
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF) Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanical.. |
|||
Melting Point | 164 - 170 °C | 327 - 338 °F | ISO 3146 |
Borealis Bormod™ HD905CF Polypropylene Homopolymer for Cast Film Bormod HD905CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, suitable for the manufacturing of unoriented film on chill roll process. It is recomme.. |
|||
Melting Point | 164 - 170 °C | 327 - 338 °F | ISO 3146 |
Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film Bormod HD915CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, especially developed for the manufacturing of unoriented film for metallizing. It is s.. |
|||
Melting Point | 164 °C | 327 °F | by DSC |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Melting Point | 164 °C | 327 °F | by DSC |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Melting Point | 164 - 168 °C | 327 - 334 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |
|||
Melting Point | 164 - 168 °C | 327 - 334 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) at 50% RH Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction prope.. |
|||
Melting Point | 164 °C | 327 °F | ISO 3146 |
Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Melting Point | 164 °C | 327 °F | ISO 3146 |
Total PPH 5060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 5060 is homopolymer.ApplicationATOFINA Polypropylene PPH 5060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 5060 is.. |
|||
Melting Point | 164 °C | 327 °F | ISO 3146 |
Total PPH 5069 Polypropylene Homopolymer, Fiber Polypropylene PPH 5069 is a homopolymer polypropylene with a Melt Flow index of 6 g/10 min.Polypropylene PPH 5069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Melting Point | 164 °C | 327 °F | DSC |
CPC - Vycom PROTEC® Copolymer Polypropylene (CPP) Protec CP is one of various types of "impact copolymers"—a rapidly growing segment of the thermoplastic sheet market. In contrast to homopolymer polypropylene (which involves the polymerization of .. |
|||
Melting Point | 164 °C | 327 °F | DSC |
CPC - Vycom PROTEC® Homopolymer Polypropylene Protec HP is a high corrosion resistant polypropylene material which exhibits excellent tensile strength and stiffness at elevated temperatures. Homopolymer polypropylene possesses excellent resista.. |
|||
Melting Point | 164 °C | 327 °F | DSC; Dow Method |
Braskem INSPIRE™ 114 Performance Polypropylene Polymer OverviewHigh melt strengthHigh toughnessExcellent processabilityHigh impact and puncture resistanceHigh film stiffness/machinabilityHigh heat resistanceComplies with U.S. FDA FCN 843, Europe EU-Dire.. |
|||
Melting Point | 164 - 167 °C | 327 - 333 °F | 10°C/min.; ISO 3146 |
Azoty Tarnow™ TARNOFORM 500 HI4 POM Easy flow high impact grade, possessing also high damping capacityInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 164 °C | 327 °F | by DSC |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Melting Point | 164 °C | 327 °F | DSC |
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr.. |
|||
Melting Point | 164 °C | 327 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |