Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 9 Sn-Pb-In Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 9 Sn-Pb-In Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose solder in 160° C range with good physical properties.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.79 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 12

@Load 100 kg,
Time 30.0 sec
12

@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 36.7 MPa
5320 psi
Elongation at Break 135.5 %
135.5 %
Shear Strength 28.9 MPa
4190 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 24.0 µm/m-°C

@Temperature 20.0 °C
13.3 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 45.0 W/m-K

@Temperature 85.0 °C
312 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 154 - 167 °C
309 - 333 °F
Solidus 154 °C
309 °F
Liquidus 167 °C
333 °F
Component Elements Properties Metric English Comments
Indium, In 12 %
12 %
Lead, Pb 18 %
18 %
Tin, Sn 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000140 ohm-cm
0.0000140 ohm-cm
Users viewing this material also viewed the following: