Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 120 - 125 °C | 248 - 257 °F | |
Oceanchem Group 2,2-Dibromo-3-nitrilopropionamide (DBNPA) Molecular Formula: C3H2Br2N2OCas No.: 10222-01-2Features: DBNPA is white crystal powder, may dissolve in acetone, polyethylene glycol, benzene, ethanol, etc, organic solvent, slightly dissolved in w.. |
|||
Melting Point | 120 °C | 248 °F | ASTM D4591 |
3M Dyneon™ THV 220A Fluorothermoplastic
(discontinued **) THV 220A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate. It is soluble in ketones, esters, or ether.. |
|||
Melting Point | 120 - 152 °C | 248 - 306 °F | |
Indium Corp. Indalloy 89 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 120 - 167 °C | 248 - 333 °F | |
Indium Corp. Indalloy 98 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 120 - 130 °C | 248 - 266 °F | |
LG Chemical LUTENE XL8080NT PE Compound Description: LUTENE XL8080NT is a standard version having excellent electrical properties for medium and high voltage power cable insulation and has a very low level of contamination.Applications: M.. |
|||
Melting Point | 120 °C | 248 °F | DIN EN ISO 314 |
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera.. |
|||
Melting Point | 120 °C | 248 °F | ASTM D3418 |
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo.. |
|||
Melting Point | 120 - 135 °C | 248 - 275 °F | |
DayGlo ZQ Pigments ZQ-17 Saturn Yellow DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 120 - 135 °C | 248 - 275 °F | |
DayGlo ZQ Pigments ZQ-21 Corona Magenta DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 120 °C | 248 °F | Dow Method (DSC) |
Dow FLEXOMER™ ETS-9078 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9078 NT 7 is intended primarily for slot cast extrusion. This narrow molecular weight distribution resin has outstanding drawdown properties and produces low modulus cast films, high.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 A 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 D 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 A 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 K 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Melting Point | 120 °C | 248 °F | DSC |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai.. |