Material Notes:
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce thickness in multi-layer films or pipesIncrease elongation resistance in polyolefin fibersAct as a nucleating agent in polyolefinsEnhance creep resistance in pipesReinforce strain hardening in polyolefinsImprove compatibility between different polymersIncrease oxidation resistance in polyolefinsInformation provided by Addcomp Polymer Additive Solutions
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 - 44.0 MPa
5950 - 6380 psi
Elongation at Break 6.0 - 15 %
6.0 - 15 %
Tensile Modulus 2.10 - 2.45 GPa
305 - 355 ksi
Thermal Properties Metric English Comments
Melting Point 162 - 167 °C
324 - 333 °F
Crystallization Temperature 116 - 122 °C
241 - 252 °F
Deflection Temperature at 0.46 MPa (66 psi) 127 - 131 °C
261 - 268 °F
Descriptive Properties Value Comments
Oxygen induction time >60 min