Braskem F7018 LDPE Injection Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem F7018 LDPE Injection Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
F7018 is a low-density polyethylene with excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating, injection molding of general purpose parts, and masterbatches.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM-D792
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 43
43
ASTM-D2240
Tensile Strength at Break 9.00 MPa
1310 psi
ASTM-D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM-D638
Film Elongation at Break, MD 390 %
390 %
ASTM-D882
Film Elongation at Break, TD 900 %
900 %
ASTM-D882
Flexural Modulus, 1% Secant 80.0 MPa
11600 psi
Blown Film Properties; ASTM-D2457
240 MPa
34800 psi
Plaque Properties; ASTM-D790
Elmendorf Tear Strength TD 55 g
55 g
ASTM-D1922
Dart Drop Test 90.0 g
0.198 lb
ASTM-D1709
Film Tensile Strength at Break, MD 25.0 MPa
3630 psi
ASTM-D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM-D882
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C

@Load 1.02 kg
187 °F

@Load 2.25 lb
ASTM-D1525
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM-D1003
Gloss 78 %
78 %
Angle 60°; ASTM-D2457
Descriptive Properties Value Comments
Temperature Profile (°C) 130-180
Injection Molding
180-310
Extrusion Coating