Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Acrylic Acid
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
7 wt% Acrylic Acid.Nucrel® 30707HS is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins.Features/Benefits: Low seal initiation temperature allows high-speed packaging. Very good hot tack, seal through contamination, and heat seal strength provides strong, reliable heat seals. Balanced acid content (7% AA) provides good adhesion to both aluminum foil and low-density polyethylene (LDPE). In extrusion coating applications, 7 MFI provides better performance in internally deckled dies compared to higher MFI extrusion coating resins. Higher drawability for thinner coatings and/or higher extrusion speeds.Typical Applications: Cable shield wrap. Sealants for sachets in both food and nonfood applications. Toothpaste tubes, as a foil/LDPE tie layer. Other foil-containing pouches and sachets. Medical/pharmaceutical packaging.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Seal Strength 1800 g/25 mm
1800 g/in
seal bar 150°C.
Hot Tack Strength 1250 g/25 mm
1250 g/in
seal bar 110°C; Packforsk method.
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
102 °C
216 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 290 °C
554 °F
Typical Die Temp. for Extrusion Coating
Melt Temperature 220 - 305 °C
428 - 581 °F
Extrusion Coating