Material Notes:
Description: Terblend® N NM-13 is ABS/PA blend combining excellent impact strength at low temperatures with easy processability and good surface appearance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.1 %
1.1 %
23°C/50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 2577
Melt Flow 26.75 g/10 min

@Load 10.0 kg,
Temperature 240 °C
26.75 g/10 min

@Load 22.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ISO 2039-2
Thermal Properties Metric English Comments
Vicat Softening Point 91.0 °C
196 °F
VST/B/50; ISO 306
165 °C
329 °F
VST/A/50; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Dielectric Constant 3.3

@Frequency 1.00e+6 Hz
3.3

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.055

@Frequency 1.00e+6 Hz
0.055

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 240 - 270 °C
464 - 518 °F
Injection Molding
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Injection Molding
Descriptive Properties Value Comments
Color Natural
Commercial Status Europe
Primary Processing Technique Injection Molding and Extrusion