Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 130 kN/m | 742 pli | Die C; ASTM D624 |
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Tear Strength | 130 kN/m | 742 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go.. |
|||
Tear Strength | <= 130 kN/m | <= 742 pli | Mapal internal |
Mapal Plastics Maplon Type 3G Polypropylene Sheet Maplon type “3G†is a single layer highly polished clear sheets, with anti-blocking properties.Main advantages: High clarity and low haze, Easy to convert due to reduced blocking, High dur.. |
|||
Tear Strength | <= 130 kN/m | <= 742 pli | Mapal internal method |
Mapal Plastics Maplon Type D Polypropylene Sheet Main advantages: High clarity and medium haze, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy to convertMain disadvantages: Low scr.. |
|||
Tear Strength | 130 kN/m | 742 pli | ASTM D624 DIE C |
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance.. |
|||
Tear Strength | 130 kN/m | 742 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Tear Strength | 130 kN/m | 742 pli | ISO 34B |
Huntsman AVALON® 95 AE Thermoplastic Polyurethane Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Tear Strength | 130 kN/m | 742 pli | ISO 34B |
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate.. |
|||
Tear Strength | 130 kN/m | 742 pli | ASTM D624 |
LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, medium high modulus, UV-stabilized, mineral-filled, blow molding and extrusion grade polypropylene copolymer, excellent impact and stiffness balance, good melt st.. |
|||
Tear Strength | 130 kN/m | 742 pli | ASTM D1004 |
SK Chemicals SKYPEL M555CR Special Grade Copper Resistance SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tear Strength | 130 kN/m | 742 pli | DIN 53515 |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 130 - 200 kN/m | 742 - 1140 pli | |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |
|||
Tear Strength | 130 kN/m | 742 pli | ISO 34 |
Chengdu Polyster H4543B Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ b.. |
|||
Tear Strength | 130 kN/m | 742 pli | ISO 34 |
Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE) Medium-low modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of low and high temperature properties. Applications requiring high original color retentio.. |
|||
Tear Strength | 130 kN/m | 742 pli | DIN ISO 34-1/Bb |
BASF Elastollan C 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tear Strength | >= 130 kN/m | >= 742 pli | ISO 34 |
Austin Novel Materials Texalan® 298A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tear Strength | 130 kN/m | 742 pli | DIN ISO 34-1/Bb |
BASF Elastollan 664 DU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | >= 130 kN/m | >= 742 pli | ISO 34 |
Austin Novel Materials Texalan® 664D Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 130 kN/m | 742 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1595 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 130 - 230 kN/m | 742 - 1310 pli | Average value: 180 kN/m Grade Count:4 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |