Mechanical Properties Metric English Comments
Tear Strength 130 kN/m
742 pli
Die C; ASTM D624
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical  (discontinued **)
This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r..
Tear Strength 130 kN/m
742 pli
ASTM D624 (Die C)
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and go..
Tear Strength 130 kN/m
740 pli
ASTM D624
Huntsman IROGRAN® A 92 K 5031 TPU-High Temperature Performance
Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov..
Tear Strength <= 130 kN/m
<= 742 pli
Mapal internal
Mapal Plastics Maplon Type 3G Polypropylene Sheet
Maplon type “3G” is a single layer highly polished clear sheets, with anti-blocking properties.Main advantages: High clarity and low haze, Easy to convert due to reduced blocking, High dur..
Tear Strength <= 130 kN/m
<= 742 pli
Mapal internal method
Mapal Plastics Maplon Type D Polypropylene Sheet
Main advantages: High clarity and medium haze, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy to convertMain disadvantages: Low scr..
Tear Strength 130 kN/m
740 pli
ISO 34-1B
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr..
Tear Strength 130 kN/m
742 pli
ASTM D624 DIE C
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer
Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance..
Tear Strength 130 kN/m
742 pli
ASTM D624 (Die C)
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer
PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel..
Tear Strength 130 kN/m
742 pli
ISO 34B
Huntsman AVALON® 95 AE Thermoplastic Polyurethane
Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Tear Strength 130 kN/m
742 pli
ISO 34B
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane
Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate..
Tear Strength 130 kN/m
740 pli
ASTM D624
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h..
Tear Strength 130 kN/m
742 pli
ASTM D624
LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate
Key Features: fractional melt flow, medium high modulus, UV-stabilized, mineral-filled, blow molding and extrusion grade polypropylene copolymer, excellent impact and stiffness balance, good melt st..
Tear Strength 130 kN/m
742 pli
ASTM D1004
SK Chemicals SKYPEL M555CR Special Grade Copper Resistance
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tear Strength 130 kN/m
742 pli
DIN 53515
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 130 - 200 kN/m
742 - 1140 pli
Goodfellow Polyvinyl Fluoride (PVF) Film
A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v..
Tear Strength 130 kN/m
742 pli
ISO 34
Chengdu Polyster H4543B Thermoplastic Polyether-ester Elastomer (TPEE)
Low modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ b..
Tear Strength 130 kN/m
742 pli
ISO 34
Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE)
Medium-low modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of low and high temperature properties. Applications requiring high original color retentio..
Tear Strength 130 kN/m
742 pli
DIN ISO 34-1/Bb
BASF Elastollan C 98 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Tear Strength >= 130 kN/m
>= 742 pli
ISO 34
Austin Novel Materials Texalan® 298A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tear Strength 130 kN/m
742 pli
DIN ISO 34-1/Bb
BASF Elastollan 664 DU TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tear Strength >= 130 kN/m
>= 742 pli
ISO 34
Austin Novel Materials Texalan® 664D Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tear Strength 130 kN/m
742 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-1595 Polyester Based TPU
Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 130 - 230 kN/m
742 - 1310 pli
Average value: 180 kN/m Grade Count:4
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..