Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium-low modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of low and high temperature properties. Applications requiring high original color retention. Molded and injected products for consumer use, such as airbag door covers, railway tie pads, seals, antenna of automobile and of mobile phone.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Melt Flow 8.0 - 13 g/10 min
8.0 - 13 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ISO 868
Tensile Strength, Ultimate 30.0 MPa
4350 psi
ISO 527-1
Elongation at Break 480 %
480 %
ISO 527-1
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Tear Strength 130 kN/m
742 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 194 °C
381 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974
Copyright © lookpolymers.com All Rights Reserved