Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: fractional melt flow, medium high modulus, UV-stabilized, mineral-filled, blow molding and extrusion grade polypropylene copolymer, excellent impact and stiffness balance, good melt strength, good processability, good weatherabilityApplications: blow molded automotive ductwork, extruded sheet and profilesDescription: Astryn BE17FC fractional melt flow, UV-stabilized, precolored, 40% calcium carbonate-filled polypropylene copolymer is designed for a variety of extrusion and blow molding applications. It is characterized by an excellent balance of properties.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792B
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 84
84
ASTM D785
Hardness, Shore D 74
74
ASTM D785
Tensile Strength, Ultimate 21.0 MPa
3050 psi
ASTM D638
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Break 280 %
280 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790A
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM D256A
Tear Strength 130 kN/m
742 pli
ASTM D624
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ASTM D648
Users viewing this material also viewed the following: