Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 130 - 200 kN/m | 742 - 1140 pli | |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |