Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster H4543B Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H4543B Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ boots, dust cover, hose jackets, wire and cable jackets, belting, profiles and seals, etc.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Melt Flow 0.50 - 1.5 g/10 min
0.50 - 1.5 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ISO 868
Tensile Strength, Ultimate 26.0 MPa
3770 psi
ISO 527-1
Elongation at Break 380 %
380 %
ISO 527-1
Flexural Modulus 0.0860 GPa
12.5 ksi
ISO 178
Tear Strength 130 kN/m
742 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 192 °C
378 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974
Copyright © lookpolymers.com All Rights Reserved