Mechanical Properties Metric English Comments
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
PolyOne Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC
LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention ..
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
PolyOne LubriOne™ PC-30CF/20T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr..
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Flexural Modulus 16.5 GPa
2390 ksi
Lehmann & Voss LUVOCOM® 50-7807 Polycarbonate, with carbon fiber and demolding aid
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl..
Flexural Modulus 16.5 GPa
2390 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon OX92182 PPS (Europe-Africa-Middle East)
LNP* STAT-KON* OX92182 is a compound based on PPS-Branched resin containing Glass Fiber, Carbon Fiber, Mineral. Added features include : Electrically Conductive.This data was supplied by SABIC-IP fo..
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific)
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 16.5 GPa
2390 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI
LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive.
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy
Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc.
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
Sumitomo Bakelite North America E 8354-19189-2 Electrical Encapsulation Grade Epoxy
Glass and mineral reinforced epoxy molding compound, formulated for the encapsulation of devices requiring high quality and thermal shock resistance.Information provided by Vyncolit, a Sumitomo Bak ..
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DE006ER PC
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific)
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
E-Polymers TEKAMID® TA250G60W , 62% Glass Fiber Reinforced PA66, DAM
High strength, weather resistanceInformation provided by E-Polymers Co. Ltd.
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 443 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.55% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 16.5 GPa
2390 ksi
ASTM D790
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)  
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
Polyram Polytron A50B01 Nylon 6.6, 50% Long Fiber Glass
50% Long fiber glass reinforced black Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram.
Flexural Modulus 16.5 GPa
2390 ksi
dry; ISO 178
DSM Novamid® MC112LG55 C10 PA6-GF55
55% Glass Reinforced
Flexural Modulus 16.5 GPa

@Temperature 23.0 °C
2390 ksi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Copyright © lookpolymers.com All Rights Reserved