Material Notes:
50% Long fiber glass reinforced black Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.0 %
1.0 %
50% RH; ISO 62
Water Absorption at Saturation 3.4 %
3.4 %
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 230 MPa
33400 psi
ISO 527
Elongation at Break 1.5 %
1.5 %
ISO 527
Tensile Modulus 18.0 GPa
2610 ksi
ISO 527
Flexural Strength 380 MPa
55100 psi
ISO 178
Flexural Modulus 16.5 GPa
2390 ksi
ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
ISO 180
Charpy Impact Unnotched 10.0 J/cm²
47.6 ft-lb/in²
ISO 179
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in