SABIC Innovative Plastics LNP STAT-KON DE006ER PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DE006ER PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption 0.140 %
0.140 %
50% RH, 24 hrs; ASTM D570
0.210 %
0.210 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm

@Time 86400 sec
0.00040 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
0.00040 - 0.0013 cm/cm

@Time 86400 sec
0.00040 - 0.0013 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0030 - 0.0040 cm/cm

@Time 86400 sec
0.0030 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
0.0035 - 0.0040 cm/cm

@Time 86400 sec
0.0035 - 0.0040 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 148 MPa
21500 psi
ISO 527
150 MPa
21800 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
1.8 %
1.8 %
ISO 527
Tensile Modulus 16.7 GPa
2420 ksi
1 mm/min; ISO 527
19.58 GPa
2840 ksi
50 mm/min; ASTM D638
Flexural Strength 220 MPa
31900 psi
ASTM D790
226 MPa
32800 psi
ISO 178
Flexural Modulus 14.54 GPa
2109 ksi
ASTM D790
16.5 GPa
2390 ksi
ISO 178
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.84 J/cm
9.07 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 9.00 J
6.64 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 27.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
27.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 143 °C

@Thickness 3.20 mm
289 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
141 °C

@Thickness 3.20 mm
286 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257