Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.5 GPa @Temperature 23.9 °C |
2400 ksi @Temperature 75.0 °F |
Dry; 8HS form; ASTM D790 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, NARC/CYDSA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ASTM D790 |
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | Crosswise; ASTM D790 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | |
Lehmann & Voss LUVOCOM® 50-7807 Polycarbonate, with carbon fiber and demolding aid Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 CF30 30% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific) LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF50 FR BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ASTM D790 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Flexural Modulus | 16.5 GPa @Temperature 23.0 °C |
2390 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |