Polymer Property : Flexural Modulus = 235 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.62 GPa
235 ksi
Tangent; ASTM D790
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.62 GPa
235 ksi
Tangent; ASTM D790
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.62 GPa
235 ksi
Tangent; ASTM D790
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.62 GPa
235 ksi
Tangent; ASTM D790
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
PolyOne Trilliant™ HC THC-01-AS149031 Trans Blue Acrylonitrile Butadiene Styrene (ABS)
Information provided by PolyOne
Flexural Modulus >= 1.62 GPa
>= 235 ksi
ASTM D790
S&E Specialty Polymers GPP1005M-EX8 PP
Application: Polypropylene compound designed with halogen-based flame retardant technology meeting the UL 94 V-2 rating.  Available in a wide range of colors and not subject to additive bloom.Info..
Flexural Modulus >= 1.62 GPa
>= 235 ksi
ASTM D790-79
S&E Specialty Polymers GPP™ 1005M-EX10 Natural PP
Application: UL94 V-2, Non-blooming flame-retardant polypropylene compound for injection moldingInformation provided by S&E Specialty Polymers
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
PolyMirae Moplen HP600N Injection Molding Grade Polypropylene
Moplen HP600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600N is a homopolymer particularly suitable for injection molding..
Flexural Modulus 1.62 GPa
235 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CH005 Polypropylene, Homopolymer, Extrusion, Strapping
COPYLENE® CH005 is a fractional melt flow polypropylene homopolymer resin available in pellet form.Information provided by Phillips 66.
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
M. Holland Company PP410 Polypropylene Homopolymer
AntistaticMedium flowGeneral purposeHomopolymerNucleatedApplications: Food containersGeneral purposeHousehold goodsToys
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
Hyosung Topilene HJ541CP PP
HJ541CP High Isostatic PP Impact CopolymerApplications:Cap of pressure bottleCharacteristics:High stiffnessSlip propertyMedium impactInformation provided by Hyosung Corporation
Flexural Modulus 1.62 GPa
235 ksi
1% Secant; ASTM D790
Flint Hills P4G4K-038 Homopolymer Polypropylene
Homopolymer, UL certified, and FDA compliant.Features: Nucleated, antistat, and clarified.Applications: Injection molding: high clarity, housewares, and syringes, for EO sterilization.Former Huntsma..
Flexural Modulus 1.62 GPa
235 ksi
ISO 178
Aardvark Polymers AARTEL® 1000 Rotational Molding Resin
Aartel 1000 is our premium grade of toughened impact modified acetal copolymer. Aartel 1000 is formulated with high impact properties combined with extended mechanical properties and elevated resist..
Flexural Modulus 1.62 GPa
235 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 0320 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.62 GPa
235 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 0320 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.62 GPa
235 ksi
5 mm/min; ISO 178
Gromax ATE70-FN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Flexural Modulus 1.62 GPa
235 ksi
5 mm/min; ISO 178
Gromax BTE45-DN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Flexural Modulus 1.62 GPa

@Temperature 23.0 °C
235 ksi

@Temperature 73.4 °F
D790B
Ineos N02J-00 Polypropylene Impact Copolymer
This is a low melt flow rate, high impact copolymer polypropylene for sheet extrusion and thick wall injection molding applications. It offers a superior balance of stiffness and impact strength fo..
Flexural Modulus 1.62 GPa
235 ksi
secant; ASTM D790
Spartech PE4130 Reinforced High Density Polyethylene Compound
Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a..
Flexural Modulus 1.62 GPa
235 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling.
Flexural Modulus 1.62 GPa
235 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ..
Flexural Modulus 1.62 GPa
235 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.
Flexural Modulus 1.62 GPa
235 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
Samyang Trimma® SD6320 PMMA, Translucent
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat..
Flexural Modulus 1.62 GPa
235 ksi
Tangent; ASTM D790
Washington Penn Medium Impact Copolymer 30% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Flexural Modulus 1.62 GPa
235 ksi
ISO 178-93
Wellman Wellamid® XT1816-BK1 Toughened Nylon 66
Description: Toughened Nylon 66Information provided by Wellman.
Flexural Modulus 1.62 GPa
235 ksi
0.1 in/min; 0.250" thickness; ASTM D-790B
Chevron Phillips EC6600 HIPS - High Impact Polystyrene
Rubber modified high impact polystyrene.Applications:Lithographic sheetPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Excellent printabilityMatte surface finishHigh hea..
Flexural Modulus 1.62 GPa
235 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
ExxonMobil Paxon™ AA60-003 Blow Molding Resin
Product Description: AA60-003 is a medium molecular weight distribution high density polyethylene which is characterized by high stiffness, excellent melt uniformity, and chemical inertness.Availabi..
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
Ineos Nova 5490 High Impact Polystyrene  (discontinued **)
High heat, Good environmental stress crack resistance, Excellent printabilityApplications: Custom sheet, Lithographic applicationsProperties were determined on injection molded specimens at 23°C an..
Flexural Modulus 1.62 GPa
235 ksi
Tangent; ASTM D790
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products.