S&E Specialty Polymers GPP1005M-EX8 PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GPP1005M-EX8 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Polypropylene compound designed with halogen-based flame retardant technology meeting the UL 94 V-2 rating.  Available in a wide range of colors and not subject to additive bloom.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.910 - 0.950 g/cc
0.910 - 0.950 g/cc
ASTM D792
Melt Flow 18 - 23 g/10 min
18 - 23 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 26.2 MPa
>= 3800 psi
ASTM D638
Elongation at Break >= 30 %
>= 30 %
ASTM D638
Flexural Modulus >= 1.62 GPa
>= 235 ksi
ASTM D790
Izod Impact, Notched >= 0.427 J/cm
>= 0.800 ft-lb/in
ASTM D256
Dart Drop, Total Energy >= 14.9 J
>= 11.0 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Flammability Test 3.0

@Thickness 1.59 mm
3.0

@Thickness 0.0625 in
Oxygen Index >= 25 %
>= 25 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 2.1

@Frequency 1000 Hz
2.1

@Frequency 1000 Hz
ASTM D1531