Material Notes:
Moplen HP600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600N is a homopolymer particularly suitable for injection molding of houseware articles, toys, packaging, closures and medical items. Moplen HP600N resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Optimized balance of stiffness and toughness; Low Warpage; Easy Processing; Excellent color and processing stability; Outstanding gloss and surface appearanceApplications: Houseware articles; Toy; Closures; Medical ItemsInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 70 %
70 %
ASTM D1003
Users viewing this material also viewed the following: