Material Notes:
Description: Toughened Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.023 cm/cm
0.023 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 527-93
Elongation at Break 100 %
100 %
ISO 527-93
Flexural Strength 65.0 MPa
9430 psi
ISO 178-93
Flexural Modulus 1.62 GPa
235 ksi
ISO 178-93
Izod Impact, Notched (ISO) 65.0 kJ/m²
30.9 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-93