Hyosung Topilene HJ541CP PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Hyosung Co.
Trade Name Topilene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene HJ541CP PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HJ541CP High Isostatic PP Impact CopolymerApplications:Cap of pressure bottleCharacteristics:High stiffnessSlip propertyMedium impactInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength, Yield 32.4 MPa
4690 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
Izod Impact, Unnotched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
0.539 J/cm

@Temperature -10.0 °C
1.01 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525