Mechanical Properties Metric English Comments
Shear Strength 19.3 MPa
2800 psi
ASTM D732
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet)
Shear Strength 19.3 MPa

@Temperature 23.0 °C
2800 psi

@Temperature 73.4 °F
Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive
Mix ratio 2 to 1 by volume.TIGA 142-EX is a medium viscosity, sag resistant epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance is desired. Thi..
Shear Strength >= 19.3 MPa
>= 2800 psi
Al/Al, bond
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System
Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien..
Shear Strength >= 19.3 MPa
>= 2800 psi
Bond, Al to Al
Master Bond EP33CLV Epoxy Resists Chemicals and High Temperatures
Description: Master Bond EP33CLV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and excel..
Shear Strength >= 19.3 MPa
>= 2800 psi
Al/Al, Tensile lap
Master Bond EP21CLV Two Component Epoxy System
Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a..
Shear Strength 19.3 MPa
2800 psi
Lap Shear; ASTM D1002
CoorsTek Epoxy Seal 216 (ES-216) B-staged epoxy lids
ES-216 is available for applications where high strength and moisture resistance are required. It displays fillet formation characteristics and, after cure, is highly temperature and moisture resist..
Shear Strength 19.3 MPa
2800 psi
Lap shear strength
BCC Products BC 5200 Kwik-Set Adhesive
BC5200 is a medium viscosity fast gelling two part Epoxy Adhesive System. With an easy to use 1 to 1 mix ratio, BC5200 is considered an excellent general purpose adhesive for in-shop use. BC5200 wil..
Shear Strength 19.3 - 19.48 MPa
2800 - 2825 psi
Tensile Shear Adhesion
3M Scotchkote™ FG 502 Epoxy Metal Repair
Scotchkote Epoxy Metal Repair FG 502 has been specifically developed as a 100% solids epoxy coating for resurfacing and reforming metal machinery and equipment. It also combines good application cha..
Shear Strength 19.3 - 19.48 MPa
2800 - 2825 psi
Tensile Shear Adhesion
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer
Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell..
Shear Strength 19.3 MPa
2800 psi
Tensile Shear Adhesion
3M Scotchkote™ HTX 517 Epoxy HT Lining
Scotchkote Epoxy HT Lining HTX 517 has been specifically developed as a 100% solids epoxy coating for resurfacing and lining equipment operating at high temperatures.Product Features:Combines good a..
Shear Strength 19.3 MPa
2800 psi
Overlap, CRS MEK/abrade/MEK
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 19.3 MPa
2800 psi
Overlap, Cold Rolled Steel
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 19.3 MPa
2800 psi
Overlap, Control
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 19.3 MPa
2800 psi
Overlap, CRS/CRS tested after RT aging
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 19.3 MPa
2800 psi
Overlap, Etched Aluminum-Cohesive Failure; ASTM D1002
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
Shear Strength 19.3 MPa
2800 psi
ASTM D1002-94
Aremco Aremco-Bond™ 526N High Performance Epoxide
Clear-Amber, 1:1 System for Tough Bonding Applications Also available filled with aluminum oxide (Alumina) or pigments
Shear Strength 19.3 MPa

@Temperature 120 - 122 °C
2800 psi

@Temperature 248 - 252 °F
Average
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
Shear Strength 19.3 MPa

@Temperature -55.0 °C
2800 psi

@Temperature -67.0 °F
Aluminum, etched, Overlap, Cohesive Failure
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of..
Shear Strength 19.3 MPa
2800 psi
Overlap, grit-blasted steel; ASTM D1002
3M Scotch-Weld™ MG1500 PR Medical Grade Instant Adhesive
3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti..
Shear Strength 19.3 MPa
2800 psi
Overlap, Aluminum; ASTM D1002-64
3M Scotch-Weld™ CA4 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Fast setting for a variety of plastics and rubbers.Information provided by 3M
Shear Strength 19.3 MPa
2800 psi
Overlap, Brass MEK/abrade/MEK
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 19.3 - 31.7 MPa
2800 - 4600 psi
Lap; ASTM D1002
3M Scotch-Weld™ RT80 Retaining Compound Anaerobic Adhesives
3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings..
Copyright © lookpolymers.com All Rights Reserved