Material Notes:
Scotchkote Epoxy HT Lining HTX 517 has been specifically developed as a 100% solids epoxy coating for resurfacing and lining equipment operating at high temperatures.Product Features:Combines good application characteristics with good corrosion and temperature resistanceDesigned for application by brush or plural feed hot sprayProvides a high build protective system capable of resisting wet heat up to 150°CPrimarily designed for resurfacing and lining metal componentsExcellent adhesion to correctly prepared metal surfaces.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thickness 762 microns
30.0 mil
Mechanical Properties Metric English Comments
Flexural Strength 66.9 MPa
9700 psi
Compressive Strength 142.9 MPa
20730 psi
post cured
Shear Strength 19.3 MPa
2800 psi
Tensile Shear Adhesion
Abrasion 0.086
0.086
[g] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
Thermal Properties Metric English Comments
Heat Distortion Temperature 149 °C
300 °F
post cured 24 hrs at 120°C
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
Touch Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Light Gray and Off White