Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mix ratio 2 to 1 by volume.TIGA 142-EX is a medium viscosity, sag resistant epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance is desired. This two to one ratio, fast setting two-part adhesive is easily mixed and cured at room temperature and develops tough, strong bonds to a wide variety of materials including stainless steel, other metals, glass ceramics and plastics. Fully cured TIGA 142-EX bonds offer superior thermal shock resistance, mechanical, electrical and impact resistant properties and low permeability to gases and vapors. The cured material has good dimensional stability and resistance to water, weather, oxygen and ozone, most petroleum products, mild acids and alkalis and many other chemicals.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
Of hardener, at 23°C
1.50 g/cc
1.50 g/cc
Of resin
Viscosity Measurement 30000
30000
Of hardener
80000
80000
Of resin
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Tensile Strength at Break 51.0 MPa
7400 psi
Elongation at Break 3.5 %
3.5 %
Tensile Modulus 2.14 GPa
310 ksi
Shear Strength 19.3 MPa

@Temperature 23.0 °C
2800 psi

@Temperature 73.4 °F
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 17.7 kV/mm
450 kV/in
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 18.0 min

@Temperature 25.0 °C
18.0 min

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Ivory
Resin
Light tan
Hardener