3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impellers, fans, valves and pipe elbows.Product Features:Designed for application by stiff brush or squeegeeProvides outstanding resistance to impingement, entrainment and erosion/corrosion.Primarily designed for resurfacing metal components used in fluid flow environments. Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thickness 254 microns
10.0 mil
Mechanical Properties Metric English Comments
Flexural Strength 62.1 MPa
9000 psi
Compressive Strength 89.6 MPa
13000 psi
Shear Strength 19.3 - 19.48 MPa
2800 - 2825 psi
Tensile Shear Adhesion
Abrasion 0.080
0.080
[g] per 1000 cycles, 1 kg, CS17 Wheel
Thermal Properties Metric English Comments
Heat Distortion Temperature 60.0 °C
140 °F
Processing Properties Metric English Comments
Cure Time 180 min
3.00 hour
Initial Set
300 min
5.00 hour
Full Mechanical
360 min
6.00 hour
Machining Time
Descriptive Properties Value Comments
Appearance Gray, Blue, Red