Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 19.3 - 19.48 MPa | 2800 - 2825 psi | Tensile Shear Adhesion |
3M Scotchkote™ FG 502 Epoxy Metal Repair Scotchkote Epoxy Metal Repair FG 502 has been specifically developed as a 100% solids epoxy coating for resurfacing and reforming metal machinery and equipment. It also combines good application cha.. |
|||
Shear Strength | 19.3 - 19.48 MPa | 2800 - 2825 psi | Tensile Shear Adhesion |
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell.. |