Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 24.1 - 31.7 MPa | 3500 - 4600 psi | |
ND Industries 541 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, cams, collars, flywheels, rotors to shaft |
|||
Shear Strength | 24.1 - 31.7 MPa | 3500 - 4600 psi | |
ND Industries 542 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, fans, cams, collars, flywheels, rotors to shaftMeets military spec Mil-R-46082B Type III |
|||
Shear Strength | 24.1 - 31.7 MPa | 3500 - 4600 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT35 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Shear Strength | 19.3 - 31.7 MPa | 2800 - 4600 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT80 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |