Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Pacific Sintered Materials FN-255-S Nickel Steel Powdered Metal Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0205-25All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0205-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
PSM Industries PolyAlloys MIM-430L sintered Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
Kobe Steel KSTI-1.5AL Alpha Titanium Alloy, Annealed Nominal Composition: Ti-1.5 Al Applications: Exhaust systems.Features:Heat resistant. Information provided by Kobe Steel |
|||
Tensile Strength, Ultimate | 345 - 517 MPa | 50000 - 75000 psi | |
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 345 - 414 MPa | 50000 - 60000 psi | |
Meehanite Almanite® W1 Wear and Abrasion Resisting Cast Iron Type W1 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W1 has a pearlitic matrix.General Meehanite information - Meehanite metal is.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Meehanite GA-50 Flake Graphite Cast Iron Type GA-50 combines high strength, toughness, wear resistance and damping capacity with excellent machinability. Responds well to heat treatment, local and surface hardening.General Meehanite infor.. |
|||
Tensile Strength, Ultimate | >= 345 MPa | >= 50000 psi | |
MetalTek AGMA CL A UNS C90800 Gear Bronze Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C90800; Cast Grade C90.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | ASTM D638 |
Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Annealed |
Special Metals Nickel 205 Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Universal Wire Works 187 Copper-Nickel Alloy Welding Wire Alloy 187 is used for arc welding of wrought or cast 70/30, 80/20, and 90/10 copper nickel alloys to themselves or to each other. Alloy 187 can be used for welding the clad side of copper-nickel cla.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Universal Wire Works 67 Nickel Alloy Welding Wire Alloy 67 is used for TIG, MIG, oxyacetylene and submerged-arc welding of 70/30, 80/20 and 90/10 copper-nickel alloys, as well as overlaying on steel. On applications using submerged-arc welding, a f.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Universal Wire Works Commercially Pure (AMS 4951) Titanium Alloy Filler Metal Universal commercially pure titanium is extremely versatile for applications requiring high temperature resistance together with resistance to many chemical reagents. Commercially pure (cp) titanium.. |
|||
Tensile Strength, Ultimate | 345 - 407 MPa | 50000 - 59000 psi | |
Eagle Brass 210 Gilding Metal, Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Premium Casting |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® D50F Silver Nickel Alloy CMW® D50F can be fabricated into wire, rod and strip; however, the headability of CMW® D50F is limited to a narrow range. It is used for main contacts in circuit breakers and switching devices whe.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 101 OFE COPPER (Certified), Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® ELKONIUM 63 Silver Alloy ELKONIUM® 63 alloy contains small amounts of magnesium and nickel. It is recommended for low voltage, vibrating contact DC applications for minimizing metal transfer. It is used in automobile volta.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | cold worked |
CMW® ELKONIUM 70 gold based alloy Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to .. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Ametek High Purity Nickel Strip 899L Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
Ametek P316L P/M Stainless Steel, Sintered from 6.30 g/cc Green Density P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu.. |
|||
Tensile Strength, Ultimate | 345 MPa @Temperature 427 °C |
50000 psi @Temperature 801 °F |
|
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allegheny Ludlum Grade 1 Titanium (UNS R50250) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allegheny Ludlum Grade 11 Titanium (UNS R52250) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | |
ATI Allegheny Ludlum Grade 17 Titanium (UNS R52252) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 345 MPa | 50000 psi | Typical |
Aleris Weldural Aluminum Alloy, 500 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |