Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 483 - 517 MPa | 70000 - 75000 psi | |
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 483 - 517 MPa | 70000 - 75000 psi | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 414 - 517 MPa | 60000 - 75000 psi | |
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 345 - 517 MPa | 50000 - 75000 psi | |
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 434 - 517 MPa | 63000 - 75000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 379 - 517 MPa | 55000 - 75000 psi | |
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Ultimate | 434 - 517 MPa | 63000 - 75000 psi | |
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 393 - 517 MPa | 57000 - 75000 psi | |
Eagle Brass 762 Nickel Silver 12%, Annealed 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Strength, Ultimate | 462 - 517 MPa | 67000 - 75000 psi | Typical |
AK Steel 18 Cr-Cb™ Ferritic Stainless steel AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili.. |
|||
Tensile Strength, Ultimate | 413 - 517 MPa | 59900 - 75000 psi | |
Ametek AM 388™ Alloy (UNS C72650) TD01 1/4 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Ultimate | 441 - 517 MPa | 64000 - 75000 psi | |
AK Steel 436L ULTRA FORM® Ferritic Stainless Steel AK Steel’s 436L ULTRA FORM® is a ferritic grade of stainless steel that outperforms Type 409 in oxidation resistance and corrosion testing. The addition of molybdenum enhances pitting resistance w.. |